Repairing Cracked Brickwork: Rebuild, or Stitch the Crack?
In my last post, I wrote about why brickwork cracks and what an articulation joint does. This post is about what happens once a wall has already cracked. In my experience, there are two ways to go.
The issue
The first is to take the cracked brickwork down and build it again. It is simple, but it is very costly, and sometimes it is not possible at all. A good deal of old brickwork was built when the site was open and easy to reach. Decades later, buildings have filled in around it, and there is no room left to set up, or to bring in bricks and sand.
The solution
The second way begins with the engineer, who assesses whether the brickwork can stay. If it is cracked but still sound, the approach changes from replacing the wall to repairing it. The method I have in mind is crack stitching: helical stainless steel bars bonded into the bed joints across the crack. Helifix is one such system used in Australia (1).

HeliBar, a helical stainless steel bar for masonry repair. Photo: Helifix.
The manufacturer describes it as a way of repairing and stabilising cracked masonry, restoring its structural integrity and spreading the load again (1). The work itself is mostly careful raking out and pointing.
Rake out the bed joint. A slot is cut along the mortar bed, in my experience about 30 to 40 mm deep. The guide sets the depth by wall thickness, from 25 to 40 mm, and runs the slot at least 500 mm past the crack on each side (1).
Clean it out. Blow out the dust, then prime the slot or flush it with water (1).
Grout and bar. A bead of grout goes to the back of the slot and the bar is pressed into it. More grout then goes over the bar, finishing 10 to 15 mm short of the face (1).
Repeat up the wall. This is usually every fourth course, about 340 mm apart. Where a thick solid wall, or both leaves of a cavity wall, have cracked, both sides are stitched (1).
Repoint and fill the crack. The bed joint is repointed and the crack itself is filled (1). On an old wall laid in lime, the new pointing should suit the old mortar, as a strong cement mix is too hard for it (2).

Pushing the bar into the grout in a raked-out bed joint. Photo: Helifix.

Crack stitching: bars go into the bed joints across the crack, then the joints are repointed. Illustration by Artvision Brickwork based on the Helifix product guide, not to scale.
In my experience, once the bars are in, the crack stops spreading. The guide describes this as minimising any further development of the crack, while the bars remain flexible enough to accommodate normal building movement (1). Because everything sits inside the joints, the repair is concealed, and the guide notes that it suits historic walls and lime mortar as well (1).
What stitching does not do is remove the cause. The manufacturer itself says that the cause should be identified first, and the repair designed to suit it (1). That is why the engineer's assessment comes before the bars, not after.
When a wall has cracked, pulling it down is not the only answer. If the engineer is satisfied that the brickwork can stay, a repair inside the joints can hold it together. These are, of course, only my own views. If you see things differently, I would like to hear from you.
artvisionbrickwork@gmail.com · Artvision Brickwork
Notes
Helifix, Product Guide: Crack Stitching and HeliBar (Australian distributor site). https://www.ancon.com.au/downloads/1971/Helifix_Product_Guide.pdf
Heritage Council of Victoria, Mortars: materials, mixes and methods. A guide to repointing mortar joints in older buildings (2021). https://assets.heritagecouncil.vic.gov.au/assets/MortarsTechnicalGuide-online.pdf




Comments