Mortar Colour Variation, Part 1: Three Common Causes

Writer: Yohan Park
Yohan Park
Nov 1
3 min read

Updated: Nov 2

Sometimes a wall is laid and cleaned, and only when you step back do you see it: the mortar is one colour for a few courses and a different colour above. Mortar colour variation has many causes. In this Part 1, I cover the three I see most often, and how I deal with it.

The issue

In my experience, the most common cause is the sand. It is ordered as the same product, but it arrives from a different batch. With an off-white cement the difference is often hard to notice. With GP (general purpose) grey cement, it shows.

A different batch matters because, as suppliers tell us, even the same product can come from a different depth in the pit, so the size and proportion of the particles in the sand can differ. Mixed with cement and water, the two batches may look almost the same colour. But once the mortar is against the brick, the curing time can be very different, and in my experience that is when colour variation is very likely to appear.

A worst case: the mortar colour changes partway up the wall. Here the bricks were from a different batch as well, not only the sand. This was one of our own Artvision jobs.

A worst case: the mortar colour changes partway up the wall. Here the bricks were from a different batch as well, not only the sand. This was one of our own Artvision jobs.

The second is laying after rain, while the sand and bricks are still wet. The extra water can turn the finished joints a yellowish colour. It is much like concrete: the more water in the mix, the paler it sets, and the weaker it is.

The third is mixing time. Mortar should turn in the mixer for at least two to three minutes. On a busy day, the sand, cement and lime can go in and come out in under a minute, straight to the bricklayers. It does not happen often, but it does happen.

The solution

The first step is to judge how big the problem is.

  • If the spare bricks cover it, meaning the wastage bricks already ordered are enough for the affected area, the first choice is to take the wall down and lay it again.

  • If they do not, and new bricks would have to be ordered, especially when that would hold up the program, bring in a specialist who can change the colour of the mortar on the finished wall, for example Ecotone or Nawkaw.

Some bricklayers may say there is a quicker way: rake out only the joints that changed colour with an Arbortech saw and fill them again. I can see why, because it looks like it would take less time. In my experience, though, the raked and refilled joints rarely match the original mortar left in the rest of the wall. To get an even colour, you would have to rake out the whole wall, fill every joint with freshly mixed mortar and joint it again. That usually takes longer than taking the wall down and laying it again. And even then, the repaired wall can end up a different colour from the walls next to it that never had a problem. For that reason, I do not recommend it.

Most of the time, though, it can be avoided. In my view, it comes down to three things:

  • Same batch of sand. Clear communication with the sand supplier, and managing the orders, so the sand for the job comes from the same batch. For example, work out the quantity accurately, then order all the sand the job needs at once and have it delivered to site. I have even had 40 m³ of sand delivered at one time to avoid this problem.

  • A plan for rain. A plan for how the materials will be managed when it rains, and actually carrying it out on site.

  • Enough mixing time. Every mix gets enough time in the mixer.

When it does happen, the next question is usually who pays for the repair. I cover that in Part 2.

These are, of course, only my own views. If you see things differently, I would like to hear from you.